Advanced alloys.
Unmatched performance.

Our superalloys make the impossible possible — delivering purity and performance that push engines higher, vehicles farther, and missions further.

Explore superalloys.

Our nickel-based and cobalt-base superalloys are engineered for pushing performance boundaries.

Thank you! Your submission has been received!
Oops! Something went wrong while submitting the form.
Nominal Chemistry
Rhenium
% Wt
10
10
Hafnium
% Wt
10
10
Tantalum
% Wt
10
10
Tungsten
% Wt
10
10
Molybdenum
% Wt
10
10
Chromium
% Wt
10
10
Nickel
% Wt
10
10
Cobalt
% Wt
10
10
Thank you! Your submission has been received!
Oops! Something went wrong while submitting the form.
Powder Alloy

1.2709 (MS1)

1.2709 (MS1) is a maraging steel powder for additive manufacturing, with ultra-high strength after age hardening for tooling and aerospace parts.
industries
Aerospace
Military & Defense
General Industrial
Space Exploration
Power Generation
SPECIFICATION
ASTM A646 / AMS 6514 / 1.2709
18
4.8
8.5
Powder Alloy

17-4PH

17-4PH is a precipitation-hardening stainless steel powder with high strength and good corrosion resistance for additively manufactured parts.
industries
Aerospace
Military & Defense
General Industrial
Power Generation
Space Exploration
SPECIFICATION
UNS S17400
4
16.5
Powder Alloy

316L

316L is a low-carbon austenitic stainless steel powder with excellent corrosion resistance for additively manufactured industrial and marine hardware.
industries
Military & Defense
Power Generation
General Industrial
Space Exploration
Aerospace
SPECIFICATION
ASTM A276 / (DIN EN 10088) 1.4404
12
17
2.5
Powder Alloy

415 SS

415 SS is a martensitic stainless steel powder with good strength and wear resistance for additively manufactured valve bodies and industrial parts.
industries
Power Generation
General Industrial
Aerospace
Military & Defense
Space Exploration
SPECIFICATION
ASTM F3056 / ASTM B446 / AISI 415
4.5
12.5
0.8
Powder Alloy

625LFe

625LFe is an iron-bearing alloy 625 variant for additive manufacturing, offering corrosion resistance and strength for industrial components.
industries
Automotive
General Industrial
Power Generation
Military & Defense
Space Exploration
SPECIFICATION
50
22
9
Powder Alloy

625 XP

625 XP is a weldable nickel-base superalloy powder for high-strength, corrosion-resistant parts up to 1093°C (2000°F).
industries
Aerospace
Power Generation
Military & Defense
Space Exploration
General Industrial
SPECIFICATION
AMS 7001 / 2.4856 / UNS N06625
50
22
9
0
0
0
0
Powder Alloy

718 XP

718 XP is a weldable nickel-base superalloy powder for high-strength, fatigue- and creep-resistant parts up to 704°C (1300°F).
industries
Aerospace
Power Generation
Military & Defense
Space Exploration
General Industrial
SPECIFICATION
ASTM F3055 / ASTM B637 / AMS 7006
52.5
19
3
0
0
0
0
Powder Alloy

939

939 is a nickel-base superalloy powder for additive manufacturing of industrial gas turbine vanes and blades requiring hot corrosion resistance.
industries
Aerospace
Power Generation
General Industrial
Military & Defense
Space Exploration
SPECIFICATION
50
22.5
1
1.4
19
Cast Alloy

AM1

AM1 is a first-generation single crystal nickel-base superalloy for high-pressure turbine blades up to approximately 1050°C.
industries
Aerospace
Military & Defense
Space Exploration
General Industrial
Power Generation
SPECIFICATION
50
8
2
6
8
6
Cast Alloy

B-1900

B-1900 is a precipitation-hardened nickel-base superalloy for conventionally cast turbine airfoils up to approximately 980°C.
industries
Aerospace
Power Generation
Military & Defense
General Industrial
Space Exploration
SPECIFICATION
AMS 5405
50
8
6
4
10
Cast Alloy

B-1900 + Hf

B-1900 + Hf is a hafnium-modified cast superalloy with improved oxidation resistance and ductility for turbine blades and vanes.
industries
Aerospace
Power Generation
Military & Defense
General Industrial
Space Exploration
SPECIFICATION
50
8
6
4
1.5
10
Cast Alloy

C1023

C1023 is a nickel-base superalloy qualified for cast aero-engine turbine blades and vanes with reliable high-temperature strength.
industries
Aerospace
Power Generation
Military & Defense
General Industrial
Space Exploration
SPECIFICATION
50
15.5
8.5
10
Cast Alloy

C263

C263 is a precipitation-hardened nickel-base alloy for combustion hardware, transition ducts, and turbine casings up to 850°C.
industries
Aerospace
Power Generation
General Industrial
Military & Defense
Space Exploration
SPECIFICATION
50
20
6
20
Cast Alloy

Co 21

Co 21 is a solid-solution cobalt-base superalloy for gas turbine nozzle vanes and combustion components requiring hot corrosion resistance.
industries
Aerospace
Power Generation
General Industrial
Military & Defense
Space Exploration
SPECIFICATION
AMS 5385
3
27
5
50
Cast Alloy

Co 25; L-605

L-605 is a cobalt-base superalloy for turbine vanes, combustion liners, and afterburner components with good oxidation resistance.
industries
Aerospace
Power Generation
Military & Defense
General Industrial
Space Exploration
SPECIFICATION
10
20
15
50
Cast Alloy

ECY 768

ECY 768 is a cast cobalt-base superalloy for first-stage gas turbine nozzle vanes with solid-solution strengthening and corrosion resistance.
industries
Aerospace
Power Generation
General Industrial
Military & Defense
Space Exploration
SPECIFICATION
10
23
7
3.5
50
Cast Alloy

FSX-414 (VAC)

FSX-414 is a cast cobalt-base superalloy for gas turbine nozzle vanes and combustion components with strong hot corrosion resistance.
industries
Aerospace
Power Generation
Military & Defense
General Industrial
Space Exploration
SPECIFICATION
10
29
7.5
50
Cast Alloy

GMR 235

GMR 235 is a nickel-base cast superalloy for turbine vane and nozzle applications in jet and industrial gas turbine engines.
industries
Aerospace
Power Generation
General Industrial
Military & Defense
Space Exploration
SPECIFICATION
50
15.5
5.3
Cast Alloy

GTD 111

GTD 111 is a nickel-base superalloy developed by GE for equiaxed and DS turbine blades in advanced industrial gas turbines.
industries
Aerospace
Power Generation
General Industrial
Space Exploration
Military & Defense
SPECIFICATION
50
14
1.5
3.7
3
9.4
Powder Alloy

HS31-X40

HS31-X40 is a cobalt-base superalloy powder for additively manufactured turbine nozzle vanes and hot-section hardware with hot corrosion resistance.
industries
Aerospace
Power Generation
Military & Defense
General Industrial
Space Exploration
SPECIFICATION
10.5
22
7.5
50
Cast Alloy

IN 100

SeAH IN 100 is a low-density, precipitation-hardenable superalloy for conventionally cast components up to 980°C.
industries
General Industrial
Space Exploration
Aerospace
Military & Defense
Power Generation
SPECIFICATION
AMS 5397
50
10
3
15
Cast Alloy

IN 625

IN 625 is a weldable nickel-base superalloy used for conventionally cast structural components up to 980°C.
industries
Aerospace
Power Generation
Military & Defense
General Industrial
Space Exploration
SPECIFICATION
AMS 5401
50
21.5
9
Cast Alloy

IN 713C

SeAH IN 713C is a precipitation-hardened superalloy for conventionally cast, solid low-pressure turbine airfoils operating at 790 to 870°C.
industries
Power Generation
Space Exploration
Aerospace
General Industrial
SPECIFICATION
AMS 5391
50
12.5
4.2
Cast Alloy

IN 713 LC

IN 713 LC is a low-carbon nickel-base cast superalloy for turbine airfoils with improved weldability and elevated-temperature strength.
industries
Aerospace
Power Generation
Military & Defense
Space Exploration
General Industrial
SPECIFICATION
AMS 5377
50
12
4.5
Cast Alloy

IN 718

IN 718 is a weldable nickel-base superalloy used for conventionally cast structural components up to 650°C.
industries
Aerospace
Power Generation
Military & Defense
General Industrial
Space Exploration
SPECIFICATION
AMS 5383
52.5
19
3
Cast Alloy

IN 738C

IN 738C is a precipitation-hardened nickel-base superalloy with good hot corrosion resistance for industrial gas turbine blades and vanes.
industries
Aerospace
Power Generation
Military & Defense
General Industrial
Space Exploration
SPECIFICATION
50
16
1.75
2.6
1.75
8.5
Cast Alloy

IN 738 LC

IN 738 LC is a nickel-base superalloy for cast turbine blades and vanes, with enhanced hot corrosion resistance and weldability up to 980°C.
industries
Aerospace
Power Generation
Military & Defense
General Industrial
Space Exploration
SPECIFICATION
AMS 5410
50
16
1.7
2.5
1.7
8.4
Cast Alloy

IN 792 + Hf

IN 792 + Hf is a hafnium-modified nickel-base superalloy with enhanced ductility and oxidation resistance for DS and cast turbine blades.
industries
Aerospace
Power Generation
Military & Defense
General Industrial
Space Exploration
SPECIFICATION
50
12.2
2
3.8
4
0.6
9
Cast Alloy

IN 939

IN 939 is a nickel-base superalloy for industrial gas turbine vanes and blades requiring hot corrosion resistance at high temperatures.
industries
Aerospace
Power Generation
General Industrial
Military & Defense
Space Exploration
SPECIFICATION
50
22.4
1.6
1.4
19
Powder Alloy

M300

M300 is an age-hardenable maraging steel powder for additively manufactured high-performance tooling, structural brackets, and aerospace components.
industries
Aerospace
Automotive
Military & Defense
General Industrial
Space Exploration
SPECIFICATION
ASTM A646 / AMS 6514
18
4.8
8.5
Cast Alloy

MAR M 002

MAR M 002 is a directionally solidified nickel-base superalloy with high creep strength and oxidation resistance for DS turbine blades.
industries
Aerospace
Power Generation
Military & Defense
General Industrial
Space Exploration
SPECIFICATION
50
9
10
2.6
1.5
10
Cast Alloy

MAR M 004

MAR M 004 is a nickel-base cast superalloy for turbine blades and vanes with balanced creep strength and oxidation resistance.
industries
Aerospace
Power Generation
Military & Defense
General Industrial
Space Exploration
SPECIFICATION
50
12
4.5
1.3
Cast Alloy

MAR M 200 + Hf

MAR M 200 + Hf is a hafnium-modified DS alloy based on MAR M 200 with improved grain boundary ductility for DS turbine blades.
industries
Aerospace
Power Generation
Military & Defense
General Industrial
Space Exploration
SPECIFICATION
50
9
12
2
10
Cast Alloy

MAR M 246

MAR M 246 is a nickel-base cast superalloy for aerospace turbine blades and vanes requiring high creep strength and hot-section durability.
industries
Aerospace
Power Generation
Military & Defense
General Industrial
Space Exploration
SPECIFICATION
50
9
2.5
10
1.5
10
Cast Alloy

Mar M 247

MAR M 247 is a high creep strength alloy used in conventionally cast gas turbine blades, vanes, and structural components from 980°C to 1010°C.
industries
Aerospace
Power Generation
General Industrial
Military & Defense
Space Exploration
SPECIFICATION
50
8
0.6
10
3
1.5
10
Powder Alloy

Mar M 247

Mar M 247 is a nickel-base superalloy powder for additively manufactured turbine blades and vanes with high creep and oxidation resistance to 1010°C.
industries
Aerospace
Power Generation
Military & Defense
General Industrial
Space Exploration
SPECIFICATION
50
8
9.5
9
Cast Alloy

MAR M 509

MAR M 509 is a cast cobalt-base superalloy for turbine nozzle vanes and hot-section components with long-duration oxidation resistance.
industries
Aerospace
Power Generation
Military & Defense
General Industrial
Space Exploration
SPECIFICATION
10
23.5
7
3.5
50
Cast Alloy

MM247LC (René 108)

R108 alloy (aka 247LC) is a modified chemistry of MAR M 247 alloy, developed for improved castability during directional solidification (DS).
industries
Aerospace
Military & Defense
Space Exploration
General Industrial
Power Generation
SPECIFICATION
50
8
0.5
10
3.2
1.4
9
Cast Alloy

Ni X

Ni X is a solid-solution strengthened nickel-base superalloy for turbine discs, shafts, and industrial hardware in high-temperature environments.
industries
Aerospace
Power Generation
Military & Defense
General Industrial
Space Exploration
SPECIFICATION
AMS 5390
50
22
9
0.6
1.5
Powder Alloy

NiX XP

NiX XP is a non-magnetic, nickel-base superalloy powder for high-strength, heat- and corrosion-resistant parts up to 1204°C (2200°F).
industries
Aerospace
Power Generation
Military & Defense
Space Exploration
General Industrial
SPECIFICATION
AMS 7008
50
22
9
0.7
0
0
1.5
Cast Alloy

PWA 1480

PWA 1480 is a first-generation single crystal nickel-base superalloy developed by Pratt and Whitney for high-pressure turbine blades.
industries
Aerospace
Military & Defense
Space Exploration
General Industrial
Power Generation
SPECIFICATION
50
10
4
12
5
Cast Alloy

PWA 1484

PWA 1484 is a second-generation rhenium-bearing single crystal nickel-base superalloy for high-pressure turbine blades.
industries
Aerospace
Military & Defense
Space Exploration
General Industrial
Power Generation
SPECIFICATION
50
5
1.9
5.9
8.7
0.1
3
10
Cast Alloy

René 125

René 125 is a nickel-base cast superalloy with good creep and oxidation resistance for first-stage turbine vanes and blades.
industries
Aerospace
Power Generation
Military & Defense
General Industrial
Space Exploration
SPECIFICATION
50
9
2
7
3.8
1.5
10
Cast Alloy

René 220

René 220 is a nickel-base cast superalloy for later-stage turbine blades and vanes requiring hot corrosion resistance.
industries
Aerospace
Power Generation
General Industrial
Military & Defense
Space Exploration
SPECIFICATION
50
18
3
3
12
Cast Alloy

René 41

René 41 is a precipitation-hardened nickel-base superalloy with excellent strength and oxidation resistance to 870°C for aerospace hardware.
industries
Aerospace
Military & Defense
Space Exploration
General Industrial
Power Generation
SPECIFICATION
AMS 5399
50
19
9.8
11
Cast Alloy

René 77

René 77 is a precipitation-hardened nickel-base cast superalloy for turbine blades and vanes with balanced creep strength and oxidation resistance.
industries
Aerospace
Power Generation
Military & Defense
General Industrial
Space Exploration
SPECIFICATION
50
15
4.2
15
Cast Alloy

René 80

René 80 is a precipitation-hardened nickel-base cast superalloy for turbine blades and vanes in aircraft engines and industrial gas turbines.
industries
Aerospace
Power Generation
Military & Defense
General Industrial
Space Exploration
SPECIFICATION
50
14
4
4
9.5
Cast Alloy

René 95

René 95 is a nickel-base superalloy for high-strength turbine discs, seals, and rotating hardware in advanced gas turbine engines.
industries
Aerospace
Power Generation
Military & Defense
General Industrial
Space Exploration
SPECIFICATION
50
14
3.5
3.5
8
Cast Alloy

René N5

René N5 is a second-generation rhenium-bearing single crystal nickel-base superalloy for high-pressure turbine blades and nozzles.
industries
Aerospace
Power Generation
Military & Defense
Space Exploration
General Industrial
SPECIFICATION
50
7
1.5
5
6.5
0.15
3
7.5
Cast Alloy

René N500

René N500 is a rhenium-free single crystal nickel-base superalloy for high-pressure turbine blades and nozzle guide vanes.
industries
Aerospace
General Industrial
Military & Defense
Power Generation
Space Exploration
SPECIFICATION
50
7
2
6.3
6.6
0.15
7.5
Cast Alloy

René N515

René N515 is a reduced-rhenium single crystal nickel-base superalloy for high-pressure turbine blades and nozzle guide vanes.
industries
Aerospace
General Industrial
Military & Defense
Power Generation
Space Exploration
SPECIFICATION
50
6
2
6.3
6.5
0.6
1.5
7.5
Cast Alloy

SC 180

SC 180 is a single crystal nickel-base superalloy for high-temperature turbine blade applications in aerospace, energy, and industrial gas turbines.
industries
Aerospace
Space Exploration
General Industrial
Military & Defense
SPECIFICATION
50
5
1.5
5.5
8
0.1
3
10
Powder Alloy

SeAH N06230

SeAH N06230 is a nickel-base superalloy powder with outstanding oxidation resistance for additively manufactured combustion hardware up to 1149°C.
industries
Aerospace
Power Generation
Military & Defense
General Industrial
Space Exploration
SPECIFICATION
UNS N06230
50
22
2
14
Powder Alloy

SeAH N07208

SeAH N07208 is a gamma prime strengthened nickel-base superalloy powder with high creep strength and strong fabricability for additive manufacturing.
industries
Aerospace
General Industrial
Military & Defense
Power Generation
Automotive
Space Exploration
SPECIFICATION
50
20
8.5
10
Cast Alloy

U 500

U 500 (Udimet 500) is a precipitation-hardened nickel-base superalloy for cast turbine blades and vanes offering strength up to approximately 870°C.
industries
Aerospace
Power Generation
Military & Defense
General Industrial
Space Exploration
SPECIFICATION
AMS 5384
50
18
4
17
Cast Alloy

U 700

U 700 (Udimet 700) is a high-strength nickel-base superalloy for cast turbine blades and discs requiring high creep rupture strength.
industries
Aerospace
Power Generation
Military & Defense
General Industrial
Space Exploration
SPECIFICATION
50
15
5.25
18.5
Cast Alloy

Waspaloy

Waspaloy is an age-hardened nickel-base superalloy for turbine discs, shafts, seals, and fasteners with strength and oxidation resistance to 870°C.
industries
Aerospace
Power Generation
Military & Defense
General Industrial
Space Exploration
SPECIFICATION
50
19.5
4.2
13.5
Cast Alloy

WI-52

WI-52 is a cast cobalt-base superalloy for turbine nozzle vanes and combustion hardware requiring hot corrosion resistance.
industries
Aerospace
Power Generation
Military & Defense
General Industrial
Space Exploration
SPECIFICATION
21
11
50
Cast Alloy

X-40

X-40 (HS-31) is a cast cobalt-base superalloy for turbine nozzle vanes and combustion components with strong hot corrosion resistance.
industries
Aerospace
Power Generation
Military & Defense
General Industrial
Space Exploration
SPECIFICATION
AMS 5382
10
25
7.5
50
Cast Alloy

X-45

X-45 is a cast cobalt-base superalloy for gas turbine nozzles and vanes with solid-solution strengthening and hot corrosion resistance.
industries
Aerospace
Power Generation
Military & Defense
General Industrial
Space Exploration
SPECIFICATION
10.5
25.5
7
50
No items found
Update your search and filter options, or clear all filters

Explore Alloys

Browse our complete range of nickel- and cobalt-based superalloys, engineered for strength, purity, and reliability.

Powder Alloy

SeAH N07208

SeAH N07208 is a gamma prime strengthened nickel-base superalloy powder with high creep strength and strong fabricability for additive manufacturing.

Cast Alloy

René N515

René N515 is a reduced-rhenium single crystal nickel-base superalloy for high-pressure turbine blades and nozzle guide vanes.

C50TF130
Cast Alloy

René N500

René N500 is a rhenium-free single crystal nickel-base superalloy for high-pressure turbine blades and nozzle guide vanes.

Powder Alloy

Mar M 247

Mar M 247 is a nickel-base superalloy powder for additively manufactured turbine blades and vanes with high creep and oxidation resistance to 1010°C.

Cast Alloy

Ni X

Ni X is a solid-solution strengthened nickel-base superalloy for turbine discs, shafts, and industrial hardware in high-temperature environments.

AMS 5390
Powder Alloy

NiX XP

NiX XP is a non-magnetic, nickel-base superalloy powder for high-strength, heat- and corrosion-resistant parts up to 1204°C (2200°F).

AMS 7008
Powder Alloy

718 XP

718 XP is a weldable nickel-base superalloy powder for high-strength, fatigue- and creep-resistant parts up to 704°C (1300°F).

ASTM F3055 / ASTM B637 / AMS 7006
B50TF251
Powder Alloy

625 XP

625 XP is a weldable nickel-base superalloy powder for high-strength, corrosion-resistant parts up to 1093°C (2000°F).

AMS 7001 / 2.4856 / UNS N06625
Powder Alloy

M300

M300 is an age-hardenable maraging steel powder for additively manufactured high-performance tooling, structural brackets, and aerospace components.

ASTM A646 / AMS 6514
Powder Alloy

HS31-X40

HS31-X40 is a cobalt-base superalloy powder for additively manufactured turbine nozzle vanes and hot-section hardware with hot corrosion resistance.

B50TF185
Powder Alloy

625LFe

625LFe is an iron-bearing alloy 625 variant for additive manufacturing, offering corrosion resistance and strength for industrial components.

Powder Alloy

415 SS

415 SS is a martensitic stainless steel powder with good strength and wear resistance for additively manufactured valve bodies and industrial parts.

ASTM F3056 / ASTM B446 / AISI 415
Powder Alloy

316L

316L is a low-carbon austenitic stainless steel powder with excellent corrosion resistance for additively manufactured industrial and marine hardware.

ASTM A276 / (DIN EN 10088) 1.4404
Powder Alloy

17-4PH

17-4PH is a precipitation-hardening stainless steel powder with high strength and good corrosion resistance for additively manufactured parts.

UNS S17400
Powder Alloy

1.2709 (MS1)

1.2709 (MS1) is a maraging steel powder for additive manufacturing, with ultra-high strength after age hardening for tooling and aerospace parts.

ASTM A646 / AMS 6514 / 1.2709
Powder Alloy

939

939 is a nickel-base superalloy powder for additive manufacturing of industrial gas turbine vanes and blades requiring hot corrosion resistance.

Cast Alloy

B-1900 + Hf

B-1900 + Hf is a hafnium-modified cast superalloy with improved oxidation resistance and ductility for turbine blades and vanes.

PWA1455
Cast Alloy

B-1900

B-1900 is a precipitation-hardened nickel-base superalloy for conventionally cast turbine airfoils up to approximately 980°C.

AMS 5405
PWA663
Cast Alloy

X-45

X-45 is a cast cobalt-base superalloy for gas turbine nozzles and vanes with solid-solution strengthening and hot corrosion resistance.

Cast Alloy

X-40

X-40 (HS-31) is a cast cobalt-base superalloy for turbine nozzle vanes and combustion components with strong hot corrosion resistance.

AMS 5382
C50TF21
Cast Alloy

WI-52

WI-52 is a cast cobalt-base superalloy for turbine nozzle vanes and combustion hardware requiring hot corrosion resistance.

Cast Alloy

Waspaloy

Waspaloy is an age-hardened nickel-base superalloy for turbine discs, shafts, seals, and fasteners with strength and oxidation resistance to 870°C.

PWA652 / PWA1471
Cast Alloy

U 700

U 700 (Udimet 700) is a high-strength nickel-base superalloy for cast turbine blades and discs requiring high creep rupture strength.

PWA656 / C50TF15
Cast Alloy

U 500

U 500 (Udimet 500) is a precipitation-hardened nickel-base superalloy for cast turbine blades and vanes offering strength up to approximately 870°C.

AMS 5384
C50T39
Cast Alloy

SC 180

SC 180 is a single crystal nickel-base superalloy for high-temperature turbine blade applications in aerospace, energy, and industrial gas turbines.

EMS55465
Cast Alloy

René N5

René N5 is a second-generation rhenium-bearing single crystal nickel-base superalloy for high-pressure turbine blades and nozzles.

C50TF87
Cast Alloy

René 220

René 220 is a nickel-base cast superalloy for later-stage turbine blades and vanes requiring hot corrosion resistance.

C5DTF91 / DMD047232
Cast Alloy

René 125

René 125 is a nickel-base cast superalloy with good creep and oxidation resistance for first-stage turbine vanes and blades.

C5OTF60 / DMD 042932
Cast Alloy

René 95

René 95 is a nickel-base superalloy for high-strength turbine discs, seals, and rotating hardware in advanced gas turbine engines.

C5UFT77
Cast Alloy

René 80

René 80 is a precipitation-hardened nickel-base cast superalloy for turbine blades and vanes in aircraft engines and industrial gas turbines.

C50TF47 / C50TF28
Cast Alloy

René 77

René 77 is a precipitation-hardened nickel-base cast superalloy for turbine blades and vanes with balanced creep strength and oxidation resistance.

C50TF15 / C50T67 / DMD0437-32
Cast Alloy

René 41

René 41 is a precipitation-hardened nickel-base superalloy with excellent strength and oxidation resistance to 870°C for aerospace hardware.

AMS 5399
C50T53 / C50TF2 / EMS55380
Cast Alloy

PWA 1484

PWA 1484 is a second-generation rhenium-bearing single crystal nickel-base superalloy for high-pressure turbine blades.

PWA 1484
Cast Alloy

PWA 1480

PWA 1480 is a first-generation single crystal nickel-base superalloy developed by Pratt and Whitney for high-pressure turbine blades.

PWA 1480
Cast Alloy

MM247LC (René 108)

R108 alloy (aka 247LC) is a modified chemistry of MAR M 247 alloy, developed for improved castability during directional solidification (DS).

C50TF83
Cast Alloy

MAR M 509

MAR M 509 is a cast cobalt-base superalloy for turbine nozzle vanes and hot-section components with long-duration oxidation resistance.

PWA647 / B50TF89 / EMS55451 / DMD0401-32
Cast Alloy

Mar M 247

MAR M 247 is a high creep strength alloy used in conventionally cast gas turbine blades, vanes, and structural components from 980°C to 1010°C.

PWA1447 / PWA1489 / EMS55447 / DMD9013-32
Cast Alloy

MAR M 246

MAR M 246 is a nickel-base cast superalloy for aerospace turbine blades and vanes requiring high creep strength and hot-section durability.

MSRR7046
Cast Alloy

MAR M 200 + Hf

MAR M 200 + Hf is a hafnium-modified DS alloy based on MAR M 200 with improved grain boundary ductility for DS turbine blades.

PWA1422 / DMD0484-32
Cast Alloy

MAR M 004

MAR M 004 is a nickel-base cast superalloy for turbine blades and vanes with balanced creep strength and oxidation resistance.

EMS55437
Cast Alloy

MAR M 002

MAR M 002 is a directionally solidified nickel-base superalloy with high creep strength and oxidation resistance for DS turbine blades.

MSRR710 / MSRR7150
Cast Alloy

IN 939

IN 939 is a nickel-base superalloy for industrial gas turbine vanes and blades requiring hot corrosion resistance at high temperatures.

PWA1495
Cast Alloy

IN 792 + Hf

IN 792 + Hf is a hafnium-modified nickel-base superalloy with enhanced ductility and oxidation resistance for DS and cast turbine blades.

PWA1456 / EMS73667 / EMS55450
Cast Alloy

IN 738C

IN 738C is a precipitation-hardened nickel-base superalloy with good hot corrosion resistance for industrial gas turbine blades and vanes.

PWA1451 / B50A563 / MSRR7228 / EMS55445
Cast Alloy

IN 738 LC

IN 738 LC is a nickel-base superalloy for cast turbine blades and vanes, with enhanced hot corrosion resistance and weldability up to 980°C.

AMS 5410
MSRR7173
Cast Alloy

IN 713C

SeAH IN 713C is a precipitation-hardened superalloy for conventionally cast, solid low-pressure turbine airfoils operating at 790 to 870°C.

AMS 5391
PWA655 / EMS55371
Cast Alloy

IN 713 LC

IN 713 LC is a low-carbon nickel-base cast superalloy for turbine airfoils with improved weldability and elevated-temperature strength.

AMS 5377
B50T1239 / MSRR7048 / EMS55079 / EMS55444
Cast Alloy

IN 100

SeAH IN 100 is a low-density, precipitation-hardenable superalloy for conventionally cast components up to 980°C.

AMS 5397
PWA658 / PWA1494 / C50TF23 / MSRR7047 / EMS55089 / DMD0432-32
Cast Alloy

GMR 235

GMR 235 is a nickel-base cast superalloy for turbine vane and nozzle applications in jet and industrial gas turbine engines.

EMS73635
Cast Alloy

FSX-414 (VAC)

FSX-414 is a cast cobalt-base superalloy for gas turbine nozzle vanes and combustion components with strong hot corrosion resistance.

B50A489
Cast Alloy

ECY 768

ECY 768 is a cast cobalt-base superalloy for first-stage gas turbine nozzle vanes with solid-solution strengthening and corrosion resistance.

Cast Alloy

Co 25; L-605

L-605 is a cobalt-base superalloy for turbine vanes, combustion liners, and afterburner components with good oxidation resistance.

B50TF144
Cast Alloy

Co 21

Co 21 is a solid-solution cobalt-base superalloy for gas turbine nozzle vanes and combustion components requiring hot corrosion resistance.

AMS 5385
Cast Alloy

C1023

C1023 is a nickel-base superalloy qualified for cast aero-engine turbine blades and vanes with reliable high-temperature strength.

MSRR7046 / EMS 73669
Cast Alloy

GTD 111

GTD 111 is a nickel-base superalloy developed by GE for equiaxed and DS turbine blades in advanced industrial gas turbines.

B50A719
Cast Alloy

AM1

AM1 is a first-generation single crystal nickel-base superalloy for high-pressure turbine blades up to approximately 1050°C.

DMD0479-32
Cast Alloy

C263

C263 is a precipitation-hardened nickel-base alloy for combustion hardware, transition ducts, and turbine casings up to 850°C.

MSRR7040 / DMD0449-32
Cast Alloy

IN 718

IN 718 is a weldable nickel-base superalloy used for conventionally cast structural components up to 650°C.

AMS 5383
PWA649 / PWA1469 / PWA1490 / B50T68 / B50TF16 / MSRR7132 / EMS55422 / DMD0423-32
Powder Alloy

SeAH N06230

SeAH N06230 is a nickel-base superalloy powder with outstanding oxidation resistance for additively manufactured combustion hardware up to 1149°C.

UNS N06230
Cast Alloy

IN 625

IN 625 is a weldable nickel-base superalloy used for conventionally cast structural components up to 980°C.

AMS 5401
PWA1468 / B50TF107 / MSRR7198 / EMS55431
Thank you! We’ll get back to you soon.

We have received your message and will respond as soon as possible. We're looking forward to working with you.

Oops! Something went wrong.

Contact our team to get started.

Whether you’re in need of a trusted partner, have specific material requirements, or are facing a challenging application, our team is ready to collaborate.

Connect with us to discuss your needs and next steps.