Cast Alloy

René 125

René 125 is a high-strength precipitation-hardened alloy combining hafnium additions for improved oxidation resistance with strong gamma prime strengthening for creep rupture performance at temperatures up to approximately 980°C. Its high hafnium and tantalum content support reliable oxidation resistance and grain boundary ductility for both equiaxed and DS casting. Qualified under C50TF60 and DMD 042932, it is used for turbine vanes and blades in aerospace and military gas turbine applications.
Industry Specification
Industries
Aerospace
Power Generation
Military & Defense
General Industrial
Space Exploration

Nominal Chemistry (wt %)

René 125 is a nickel-base cast superalloy with good creep and oxidation resistance for first-stage turbine vanes and blades.
0.11
Carbon
4.8
Aluminium
0.017
Boron
9
Chromium
10
Cobalt
1.5
Hafnium
2
Molybdenum
Niobium / Columbium
3.8
Tantalum
2.5
Titanium
7
Tungsten
0.05
Zirconium
Iron
Bal
Nickel

Explore More

View All Alloys
Powder Alloy

SeAH N07208

SeAH N07208 is a gamma prime strengthened nickel-base superalloy powder with high creep strength and strong fabricability for additive manufacturing.
INDUSTRIES
Aerospace
General Industrial
Military & Defense
Power Generation
Automotive
specification
Cast Alloy

René N515

René N515 is a reduced-rhenium single crystal nickel-base superalloy for high-pressure turbine blades and nozzle guide vanes.
INDUSTRIES
Aerospace
General Industrial
Military & Defense
Power Generation
Space Exploration
specification
Cast Alloy

René N500

René N500 is a rhenium-free single crystal nickel-base superalloy for high-pressure turbine blades and nozzle guide vanes.
INDUSTRIES
Aerospace
General Industrial
Military & Defense
Power Generation
Space Exploration
specification
Cast Alloy

René 125

René 125 is a high-strength precipitation-hardened alloy combining hafnium additions for improved oxidation resistance with strong gamma prime strengthening for creep rupture performance at temperatures up to approximately 980°C. Its high hafnium and tantalum content support reliable oxidation resistance and grain boundary ductility for both equiaxed and DS casting. Qualified under C50TF60 and DMD 042932, it is used for turbine vanes and blades in aerospace and military gas turbine applications.

Keep exploring.

All alloys
Powder Alloy

SeAH N07208

SeAH N07208 is a gamma prime strengthened nickel-base superalloy powder with high creep strength and strong fabricability for additive manufacturing.

Cast Alloy

René N515

René N515 is a reduced-rhenium single crystal nickel-base superalloy for high-pressure turbine blades and nozzle guide vanes.

C50TF130
Cast Alloy

René N500

René N500 is a rhenium-free single crystal nickel-base superalloy for high-pressure turbine blades and nozzle guide vanes.