IN 100 delivers a high strength-to-weight ratio for hot-section hardware. It is used for both internally cooled and solid, uncooled turbine airfoils as well as integral wheels. Qualified to AMS 5397 and a range of OEM specifications including PWA 658 and MSRR 7047, IN 100 is optimized for conventional casting to provide reliable performance at elevated temperatures.
SeAH N07208 is a gamma prime strengthened nickel-base superalloy powder with high creep strength and strong fabricability for additive manufacturing.
Industries
AMS
OEM
René N515 is a reduced-rhenium single crystal nickel-base superalloy for high-pressure turbine blades and nozzle guide vanes.
Industries
AMS
OEM
René N500 is a rhenium-free single crystal nickel-base superalloy for high-pressure turbine blades and nozzle guide vanes.
Industries
AMS
OEM