Cast Alloy

GTD 111

GTD 111 offers a high gamma prime fraction providing strong creep and tensile strength at temperatures approaching 1000°C, with good hot corrosion resistance from its moderate chromium content. It is a production alloy for first-stage turbine blades and buckets in GE's industrial gas turbine product lines, used in both equiaxed and directionally solidified form. Qualified under B50A719, GTD 111 is a workhorse alloy for power generation and aero-derivative applications requiring dependable long-interval performance.
Industry Specification
Industries
Aerospace
Power Generation
General Industrial
Space Exploration
Military & Defense

Nominal Chemistry (wt %)

GTD 111 is a nickel-base superalloy developed by GE for equiaxed and DS turbine blades in advanced industrial gas turbines.
0.1
Carbon
3
Aluminium
0.01
Boron
14
Chromium
9.4
Cobalt
Hafnium
1.5
Molybdenum
Niobium / Columbium
3
Tantalum
5
Titanium
3.7
Tungsten
Zirconium
Iron
Bal
Nickel

Explore More

View All Alloys
Powder Alloy

SeAH N07208

SeAH N07208 is a gamma prime strengthened nickel-base superalloy powder with high creep strength and strong fabricability for additive manufacturing.
INDUSTRIES
Aerospace
General Industrial
Military & Defense
Power Generation
Automotive
specification
Cast Alloy

René N515

René N515 is a reduced-rhenium single crystal nickel-base superalloy for high-pressure turbine blades and nozzle guide vanes.
INDUSTRIES
Aerospace
General Industrial
Military & Defense
Power Generation
Space Exploration
specification
Cast Alloy

René N500

René N500 is a rhenium-free single crystal nickel-base superalloy for high-pressure turbine blades and nozzle guide vanes.
INDUSTRIES
Aerospace
General Industrial
Military & Defense
Power Generation
Space Exploration
specification
Cast Alloy

GTD 111

GTD 111 offers a high gamma prime fraction providing strong creep and tensile strength at temperatures approaching 1000°C, with good hot corrosion resistance from its moderate chromium content. It is a production alloy for first-stage turbine blades and buckets in GE's industrial gas turbine product lines, used in both equiaxed and directionally solidified form. Qualified under B50A719, GTD 111 is a workhorse alloy for power generation and aero-derivative applications requiring dependable long-interval performance.

Keep exploring.

All alloys
Powder Alloy

SeAH N07208

SeAH N07208 is a gamma prime strengthened nickel-base superalloy powder with high creep strength and strong fabricability for additive manufacturing.

Cast Alloy

René N515

René N515 is a reduced-rhenium single crystal nickel-base superalloy for high-pressure turbine blades and nozzle guide vanes.

C50TF130
Cast Alloy

René N500

René N500 is a rhenium-free single crystal nickel-base superalloy for high-pressure turbine blades and nozzle guide vanes.