René 95 is a high niobium and tungsten precipitation-hardened alloy developed for turbine discs and high-strength rotating hardware requiring excellent tensile and fatigue properties at intermediate temperatures. It is produced by powder metallurgy or cast routes for disc and structural applications where fine grain size and high strength are the primary requirements. Qualified under C5UFT77, René 95 serves aerospace and military propulsion applications requiring structural integrity under high rotational stress.
SeAH N07208 is a gamma prime strengthened nickel-base superalloy powder with high creep strength and strong fabricability for additive manufacturing.
Industries
AMS
OEM
René N515 is a reduced-rhenium single crystal nickel-base superalloy for high-pressure turbine blades and nozzle guide vanes.
Industries
AMS
OEM
René N500 is a rhenium-free single crystal nickel-base superalloy for high-pressure turbine blades and nozzle guide vanes.
Industries
AMS
OEM