Cast Alloy

IN 718

IN 718 is precipitation strengthened by gamma prime and gamma double-prime phases, providing good creep resistance and strength at intermediate temperatures. Originally developed for forged discs and structural assemblies, cast IN 718 reduces processing and waste, enables more intricate design features, and can be weld-repaired. Qualified to AMS 5383 and a wide range of OEM specifications, it is used across aerospace, defense, and industrial applications.
Industry Specification
AMS 5383
Industries
Aerospace
Power Generation
Military & Defense
General Industrial
Space Exploration

Nominal Chemistry (wt %)

IN 718 is a weldable nickel-base superalloy used for conventionally cast structural components up to 650°C.
0.06
Carbon
0.5
Aluminium
0.005
Boron
19
Chromium
Cobalt
Hafnium
3
Molybdenum
5
Niobium / Columbium
Tantalum
0.9
Titanium
Tungsten
Zirconium
Bal
Iron
52.5
Nickel

Explore More

View All Alloys
Powder Alloy

SeAH N07208

SeAH N07208 is a gamma prime strengthened nickel-base superalloy powder with high creep strength and strong fabricability for additive manufacturing.
INDUSTRIES
Aerospace
General Industrial
Military & Defense
Power Generation
Automotive
specification
Cast Alloy

René N515

René N515 is a reduced-rhenium single crystal nickel-base superalloy for high-pressure turbine blades and nozzle guide vanes.
INDUSTRIES
Aerospace
General Industrial
Military & Defense
Power Generation
Space Exploration
specification
Cast Alloy

René N500

René N500 is a rhenium-free single crystal nickel-base superalloy for high-pressure turbine blades and nozzle guide vanes.
INDUSTRIES
Aerospace
General Industrial
Military & Defense
Power Generation
Space Exploration
specification
Cast Alloy

IN 718

IN 718 is precipitation strengthened by gamma prime and gamma double-prime phases, providing good creep resistance and strength at intermediate temperatures. Originally developed for forged discs and structural assemblies, cast IN 718 reduces processing and waste, enables more intricate design features, and can be weld-repaired. Qualified to AMS 5383 and a wide range of OEM specifications, it is used across aerospace, defense, and industrial applications.

Keep exploring.

All alloys
Powder Alloy

SeAH N07208

SeAH N07208 is a gamma prime strengthened nickel-base superalloy powder with high creep strength and strong fabricability for additive manufacturing.

Cast Alloy

René N515

René N515 is a reduced-rhenium single crystal nickel-base superalloy for high-pressure turbine blades and nozzle guide vanes.

C50TF130
Cast Alloy

René N500

René N500 is a rhenium-free single crystal nickel-base superalloy for high-pressure turbine blades and nozzle guide vanes.