SC 180 is an age-hardenable single crystal alloy engineered for exceptionally high yield, tensile, and creep-rupture properties at temperatures up to 1000°C. Its grain-boundary-free single crystal structure eliminates the primary failure mechanisms of polycrystalline alloys, enabling reliable performance in the most demanding hot-section environments. Qualified under EMS 55465, SC 180 is used for high-pressure turbine blades in aerospace, space, and industrial gas turbine applications requiring maximum temperature capability.
SeAH N07208 is a gamma prime strengthened nickel-base superalloy powder with high creep strength and strong fabricability for additive manufacturing.
Industries
AMS
OEM
René N515 is a reduced-rhenium single crystal nickel-base superalloy for high-pressure turbine blades and nozzle guide vanes.
Industries
AMS
OEM
René N500 is a rhenium-free single crystal nickel-base superalloy for high-pressure turbine blades and nozzle guide vanes.
Industries
AMS
OEM