SeAH 7208 is a gamma prime strengthened nickel-base superalloy powder for additive manufacturing of high-temperature structural parts. It pairs strong creep resistance with better fabricability and resistance to strain-age cracking than most gamma prime alloys, supporting laser powder bed fusion and directed energy deposition of gas turbine combustor and exhaust hardware, casings, and ducting across aerospace, power generation, and industrial markets.
SeAH 7208 is a gamma prime strengthened nickel-base superalloy powder with high creep strength and strong fabricability for additive manufacturing.
Industries
AMS
OEM
René N515 is a reduced-rhenium single crystal nickel-base superalloy for high-pressure turbine blades and nozzle guide vanes.
Industries
AMS
OEM
René N500 is a rhenium-free single crystal nickel-base superalloy for high-pressure turbine blades and nozzle guide vanes.
Industries
AMS
OEM